FERITOVÉ JADRÁ EFD

FERITOVÉ JADRÁ EFD

product-705-272

 

MODEL

G.W

VEĽKOSŤ (mm)

A

B

C

D

C

F

G

H

EFD20

9

20.0±0.6

15.4±0.5

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21A

9

20.8±0.6

15,4 min

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21B

9.7

21.0±0.5

15,4 min

8.9±0.2

6.7±0.2

8.0±0.3

10.3±0.3

\

3.6±0.2

EFD25.6

19

25.6±0.7

19.5±0.7

11.4±0.3

9.1±0.3

9.3±0.3

12.5±0.3

0.6±0.1

5.2±0.3

EFD31

25

30.8±0.8

23,2 min

14.4±0.3

8.8±0.2

11.2±0.3

15.0±0.3

0.3±0.2

4.8±0.2

EFD34

29.6

34.0±0.6

24.0±0.5

17.0±0.3

5.0±0.2

18.0±0.3

23.0±0.3

\

3.0±0.2

EFD40/45/11

60

40.5±0.7

30.0 min

16.6±0.3

10.6±0.2

16.3±0.3

22.5±0.3

\

6.6±0.2

EFD40/44/8

44

40.0±0.7

29,5 min

19.9±0.4

8.0±0.2

17.1±0.3

22.0±0.3

\

4.0±0.2

EFD43/53/4.4

63.6

43.0±0.8

28,5 min

21.6±0.4

7.6±0.25

19.3±0.3

26.5±0.3

\

4.4±0.25

EFD43/44/3.2

49.2

43.4±0.8

33,5 min

22.3±0.4

8.0±0.25

17.1±0.3

22.2±0.3

\

3.2±0.25

EFD45/50

67

45.2±0.8

33.3±0.8

24.0±0.4

7.8±0.2

18.0±0.3

24.7±0.3

\

4.0±0.2

EFD52.5

118

52.5±1.1

39 min

22.5±0.4

13.0±0.3

19.9±0.3

27.0±0.3

\

7.5±0.3

 

MODEL

PARAMETER

AL±25%(nH/N^2)

N.W(g)

C1 mm-1

Lemm

Aemm2

Vemm3

ZP40

EFD20

1.52

47.0

31.0

1460.0

1150

7.9

EFD21A

1.57

49.3

31.0

1460.0

1400

7.9

EFD21B

1.57

49.3

31.4

1540.0

1450

8.6

EFD25.6

1.00

57.0

58.0

3300.0

2000

16.5

EFD31

0.99

68.2

69.1

4712.0

2000

23.0

EFD34

1.90

95.0

50.0

4750.0

1400

33.5

EFD40/45/11

1.02

108.8

106.5

10951.0

2300

55.0

EFD40/44/8

1.35

102.8

75.5

7750.0

1700

38.0

EFD43/53/4.4

1.14

111.3

99.8

11113.0

2000

59.0

EFD43/44/3.2

1.41

102.0

72.1

7352.0

1500

43.0

EFD45/49

1.08

108.0

97.7

10356.2

2700

60.0

EFD52.5

0.78

132.0

168.0

23250.0

2750

109.0

Populárne Tagy: feritové jadrá efd, Čína výrobcovia feritových jadier efd, dodávatelia, továreň